Skip to main content
. 2021 Jan 21;14(3):515. doi: 10.3390/ma14030515

Figure 7.

Figure 7

Comparison of degree of conversion (%) between ISO at 2 mm and 3 s group at a 2 mm depth of the top specimen (mean values ± 1 standard deviation). Brackets denote statistically similar pairs of 3 s and ISO groups of the same material (p < 0.05).