Table 4.
Sample | Element | Corrected RSF | Area | Corrected Area | Ratio (%) |
---|---|---|---|---|---|
PAR–chitosan–GO | C | 1.2070 | 16,139 | 13,371.2 | 63.51 |
O | 3.1048 | 19,169 | 6174 | 29.32 | |
N | 2.0520 | 2998 | 1461 | 6.94 | |
Co | 18.5764 | 858 | 46.2 | 0.22 |
Sample | Element | Corrected RSF | Area | Corrected Area | Ratio (%) |
---|---|---|---|---|---|
PAR–chitosan–GO | C | 1.2070 | 16,139 | 13,371.2 | 63.51 |
O | 3.1048 | 19,169 | 6174 | 29.32 | |
N | 2.0520 | 2998 | 1461 | 6.94 | |
Co | 18.5764 | 858 | 46.2 | 0.22 |