Table 7.
Sample | Element | Corrected RSF | Sub-Peak | Area | Corrected Area | Ratio (%) |
---|---|---|---|---|---|---|
CdS QD–chitosan–GO before contact with Co2+ | C | 1.2070 | C–C | 6594.5 | 5463.5 | 46.45 |
C–O, C–O–C | 5438.9 | 4506.1 | 38.31 | |||
C=O, O–C=O | 2163.6 | 1792.5 | 15.24 | |||
O | 3.1048 | O–C, C–O–C | 10,782.7 | 3472.9 | 69.57 | |
O=C | 4716.3 | 1519.0 | 30.43 | |||
N | 2.0520 | Amine | 515.9 | 251.4 | 70.01 | |
C–N | 221.1 | 107.7 | 29.91 | |||
CdS QD–chitosan–GO after contact with Co2+ | C | 1.2070 | C–C | 7542.7 | 6249.1 | 44.56 |
C–O, C–O–C | 7332.8 | 6075.2 | 43.32 | |||
C=O, O–C=O | 2051.6 | 1699.8 | 12.12 | |||
O | 3.1048 | O–C, C–O–C | 14,528.3 | 4679.3 | 73.29 | |
O=C | 5294.7 | 1705.3 | 26.71 | |||
N | 2.0520 | Amine | 935.1 | 455.7 | 67.32 | |
C–N | 453.9 | 221.2 | 32.68 |