Skip to main content
. 2020 Dec 22;13(1):370–381. doi: 10.1021/acsami.0c16253

Figure 2.

Figure 2

XRD patterns of the HNO3-washed platelets (cast on Si monocrystalline substrate) after different times of the TC reaction (200 °C, 6 M NaOH, Sr/Ti = 12).