Skip to main content
. 2021 Jan 27;22(2):949–960. doi: 10.1021/acs.biomac.0c01621

Table 1. Structure, Composition, and Thermal Properties of the Evaluated Polymerse.

3.

a

Determined by 1H NMR (CDCl3, 400 MHz).

b

Determined by SEC (CHCl3, 0.5 mL min–1) versus polystyrene standards.

c

Determined by DSC.

d

The degree of crystallinity, Xc, was calculated from DSC considering an enthalpy of fusion for an infinitely large PLLA crystal of 93 J g–1 53 and for a PCL crystal of 136.1 J g–1.54

e

Not detectable under the experimental DSC condition used.