Skip to main content
. 2021 Feb 25;16(2):e0247081. doi: 10.1371/journal.pone.0247081

Fig 7.

Fig 7

Changes in contact angle (indicative of increased surface wettability) of ASW droplets with time on Cu metal surfaces deposited with and without ASW and exposed to daily repeated dry/wet cycles for 1 day, 1, 2 and 4 weeks (a) SEM images of (b) bacteria and some corrosion products on the surface of Cu metal with deposited ASW for 1 day and (c) bacteria and corrosion products on Cu metal deposited with ASW for 4 weeks.