Skip to main content
. 2021 Feb 10;14(4):843. doi: 10.3390/ma14040843

Figure 6.

Figure 6

SEM microphotographs of the surface of composites containing 0.5 wt.% of: hss-SiO2 (A) and lss-SiO2 (B) and EDS analysis of the surface of the composite after SBF/3 days/ 37 °C.