Figure 3.

Figure 3

Destructive tests: (a) Instron 8872 machine; (b) Tensile strength testing; (c) Instron 8801 universal testing machine; (d) Compressive strength testing; (e) Cubic samples for compressive strength testing. Samples #1–#5 belong in the control group while samples #6–#10 are in the heat treatment group; (f) Heat treated samples for tensile strength testing. Samples #1–#4 and #7–#10 have undergone full heat treatment while samples #5–#6 and #11–#12 went through partial heat treatment. Samples #1–#6 are printed in horizontal orientation while #7–#12 are printed in vertical orientation; (g) Control group for tensile strength testing. Samples #13–#17 are printed in horizontal orientation while #18–#22 are printed in vertical orientation.