Skip to main content
. 2021 Feb 13;13(4):562. doi: 10.3390/polym13040562

Figure 6.

Figure 6

Compressive strength testing results: (a) Compressive strength of the 5 samples from the control group varied between 41.3 MPa and 98.4 MPa; (b) Compressive strength of the 5 samples from the heat-treated group varied between 73.4 MPa and 118.1 MPa.