Skip to main content
. 2021 Feb 13;13(4):562. doi: 10.3390/polym13040562

Figure 11.

Figure 11

Scanning Electron Microscopy image of a control sample printed in vertical orientation (sample #18): (ac) Upon rupture, the sample presented uniform fracture lines along the deposited horizontal layers, showing poor adhesion at the layer level; (df) Internal gaps between deposited filaments remained embedded in the part, weakening the structure; (gi) Bigger internal voids remained embedded in the part in the area where the raster angle changes from one layer to another.