. 2021 Feb 13;13(4):562. doi: 10.3390/polym13040562

Figure 12.

Figure 12

Scanning Electron Microscopy image of a sample printed in vertical orientation (sample #09): (ac) Unlike the control sample, the linear voids between deposited filaments have been filled during the heat treatment; (df) Upon rupture, the sample presented fracture lines along multiple horizontal layers, indicating superior layer adhesion; (gi) Spherical pockets of air 10–70 µm in diameter remain inside the part.