Skip to main content
. 2021 Feb 19;14(4):981. doi: 10.3390/ma14040981

Figure 5.

Figure 5

Figure 5

The sampling sites during demolition: Corroded steel mesh and carbonate icicles: (a) location of samples 2 and 4, (b) location of samples 2, (c) location of samples 1 and 2, (d) location of samples 3 and 4.