Skip to main content
. 2021 Feb 19;14(4):990. doi: 10.3390/ma14040990

Figure 9.

Figure 9

Energy-dispersive X-ray spectroscopy of worn surfaces composites: (a) 19.62 N, 1.30 m/s and 0% SiC; (b) 39.24 N, 1.3 m/s and 6% SiC; (c) 58.86, 2.6 m/s 9% SiC.