Skip to main content
. 2021 Mar 3;11:5075. doi: 10.1038/s41598-021-84376-6

Figure 3.

Figure 3

(a) FTIR of a nanocomposite thin film (450 nm thickness, molar ratio Si/Ti : 6/1, CoFe2O4 MNPs : 0.4 vol%) and its modification upon DUV irradiation (carried out with LC8 lamp at 70 mW/cm2). (b) Widening of the 1680–1600 cm−1 region to highlight the decrease of the C=C band (LC8 lamp at 70 mW/cm2). (c) Conversion of the C=C band plotted as a function of the irradiation time (line is for guiding eye).