Skip to main content
. 2021 Feb 5;7(1):16. doi: 10.3390/gels7010016

Table 2.

Data presenting M(T)/M0 percent and the maximum temperatures of rate decomposition (Tmax) of HNT-free hydrogel and cryogel (HNT0/PHAD-Hgs and -Cgs) and ternary hybrid hydrogel and cryogel (HNT10/PHAD and HNT11/PHAD-Hgs and -Cgs) prepared at HNT content 2.80% and 3.20% (w/v).

Sample
Designation
Tmax1
(°C)
M(T)/M0
Percent
at Tmax1
Tmax2
(°C)
M(T)/M0
Percent
at Tmax2
Residual Mass at
700 °C (%)
HNT0/PHAD-Hgs 333.4 82.3 421.5 39.2 7.2
HNT0/PHAD-Cgs 323.5 80.1 425.2 32.8 7.9
HNT10/PHAD-Hgs 322.4 86.0 428.5 47.2 26.9
HNT10/PHAD-Cgs 321.7 86.4 432.1 44.7 27.0
HNT11/PHAD-Hgs 309.1 87.4 428.7 51.2 29.8
HNT11/PHAD-Cgs - - 428.5 47.1 29.0