Skip to main content
. 2021 Feb 1;54(Pt 1):280–286. doi: 10.1107/S1600576720015885

Table 2. The 〈ρ〉 dislocation-density values obtained for the as-received, heat treated for 24 h and heat treated for 200 h at 533 ± 10 K samples.

Sample E110G 〈ρ〉 (1014 m−2)
As received 27
Heat treated for 24 h 20
Heat treated for 200 h 9