Table 2:
Surface treatment | Aging | Ra (μm) | Biaxial strength (MPa) | Monoclinic phase (vol%) |
---|---|---|---|---|
As Sintered | Baseline | 0.32 (0.10) | 908 (131) | < 1 |
Autoclave | 0.33 (0.15) | 724 (188) | ~8 | |
Thermocycling | 0.31 (0.10) | 689 (185) | ~11 | |
Grind | Baseline | 0.87 (0.16) | 1298 (194) | ~32 |
Autoclave | 1.32 (0.30) | 1009 (147) | ~33 | |
Thermocycling | 1.00 (0.19) | 926 (182) | ~31 | |
Grind + Polish | Baseline | 0.55 (0.12) | 1224 (149) | ~28 |
Autoclave | 0.43 (0.12) | 1085 (77) | ~27 | |
Thermocycling | 0.55 (0.15) | 1086(144) | ~28 |