The wound surface area was significantly reduced (P < 0·05) in the oxidised regenerated cellulose (ORC)/collagen group after 8 weeks (y‐axis: percentage wound surface reduction) when compared with the control wounds (65% ± 13 versus 41% ± 11, n = 33).