Table 3.
The amount of D149 dye loading on SANP, 18NR-Tand films (thickness = 5.0 ± 0.3 µm; Area = 1 cm2) calculated using desorption method [63]
| Photoanode | D149 loading (nmol·cm−2) | D149 loading (µmol·cm−3) | D149 loading (nm−2) |
|---|---|---|---|
| SANP | 72 ± 1.5 | 111 ± 2 | 1.8 |
| NR18-T | 65 ± 0.6 | 99 ± 1 | 1.3 |
| WER2-O | 23 ± 0.2 | 36 ± 1 | 1.3 |