Table 1.
Variables | Process parameters | Levels | ||
---|---|---|---|---|
− 1 | 0 | + 1 | ||
X1 | Areal density (grams per sq. meter (GSM)) | 40 | 60 | 80 |
X2 | Electrospinning time (hrs) | 1 | 2 | 3 |
X3 | TNT (wt%) | 5 | 10 | 15 |
Variables | Process parameters | Levels | ||
---|---|---|---|---|
− 1 | 0 | + 1 | ||
X1 | Areal density (grams per sq. meter (GSM)) | 40 | 60 | 80 |
X2 | Electrospinning time (hrs) | 1 | 2 | 3 |
X3 | TNT (wt%) | 5 | 10 | 15 |