Skip to main content
. 2021 Feb 26;14(5):1100. doi: 10.3390/ma14051100

Figure 3.

Figure 3

SEM morphologies of fractured surfaces sintered at different temperatures: (a) 1800 °C, (b) 1850 °C, (c) 1900 °C, (d) 1950 °C, (e) 2000 °C, (f) 2050 °C.