Figure 11.

Figure 11

Variation in grain size between samples welded with different rotational speeds in different weld zones compared with those of the base material: (a) batch I [50]; (b) batch II (BM – Base material; HAZ–Heat affected zone; TAMAZ–Thermo-mechanically affected zone; SZ–Stir zone).