Table 5.

The specimen thinning (measured from the macrographs as shown in Figure 14 in the middle of the stir zone for each specimen from the batch I and II and then subtracted from an initial value of specimen thickness 0.8 mm).

Specimen Thinning 4500 rpm 4000 rpm 3500 rpm 3000 rpm 2500 rpm 2000 rpm 1500 rpm 1000 rpm
Batch I (mm) 0.35 ± 0.01 0.48 ± 0.03 0.39 ± 0.02 0.32 ± 0.01 0.12 ± 0.01
(%) 43.8 ± 1.25 60 ± 3.75 48.8 ± 2.5 40 ± 2.5 15 ± 1.25
Batch II (mm) 0.19 ± 0.03 0.36 ± 0.02 0.28 ± 0.03 0.29 ± 0.01 0.26 ± 0.02 0.26 ± 0.02 0.28 ± 0.01 0.17 ± 0.01
(%) 23.8 ± 3.75 45 ± 2.5 35 ± 3.75 36.3 ± 1.25 32.5 ± 2.5 32.5 ± 2.5 35 ± 1.25 21.3 ± 1.25
Base material (mm) 0.27 ± 0.3
(%) 33.75 ± 3.75