Skip to main content
. 2021 Feb 27;13(5):740. doi: 10.3390/polym13050740

Figure 7.

Figure 7

SEM images from cryogenic fractured surface of PLA/PBAT/PBS/nano talc: (a) 70/30/0/10; (b) 70/0/30/10; (c) 70/10/20/10.