Skip to main content
. 2021 Mar 6;13(5):809. doi: 10.3390/polym13050809

Table 2.

Molar ratio of reagents adopted for the synthesis of BUMA-based polymers.

Sample <dDLS> (nm) Fox Tg (°C) Real Tg (°C)
BUMA_MA 180 ± 70 67.1 n.d.
BUMA_MA_MMA (85 ± 15); (250 ± 60) 55.5 78.2
BUMA_MA_MMA_T3 80 ± 20 55.5 75.2
BUMA_MAC_25 (37 ± 7); (170 ± 30) 40.8 46.1
BUMA_MAC_50 (25 ± 4); (80 ± 10) 71.1 51.0
BUMA_MAC_75 12 ± 3 120.3 n.d.