Table 6.
Pretreatment | |||||
---|---|---|---|---|---|
No Plating | Carbon Nanotube Dip Coating |
Graphene Dip Coating |
Aluminum Sputtering |
Palladium Activating |
|
Failure strength (MPa) | 3.63 | 9.91 | 19.31 | 8.58 | 15.05 |
Failure strain | 0.45 | 0.63 | 0.64 | 0.57 | 0.69 |
Pretreatment | |||||
---|---|---|---|---|---|
No Plating | Carbon Nanotube Dip Coating |
Graphene Dip Coating |
Aluminum Sputtering |
Palladium Activating |
|
Failure strength (MPa) | 3.63 | 9.91 | 19.31 | 8.58 | 15.05 |
Failure strain | 0.45 | 0.63 | 0.64 | 0.57 | 0.69 |