Figure 14.
Surfaces of stretched sheet of 7475 (Al–Zn-Mg-Cu) alloy heated to 515 °C (a) in air; (b) in air containing some NaBF4 [39].
Surfaces of stretched sheet of 7475 (Al–Zn-Mg-Cu) alloy heated to 515 °C (a) in air; (b) in air containing some NaBF4 [39].