Electrospinning parameters for three fiber diameters used in the study

Fiber diameter (μm) ± SD PCL (wt%) Solution and solvent ratio Needle inner diameter (mm) V source (kV) V collector (kV) Flowrate (μl/min)
1.60 ± 0.26 (thin) 12 6:1 CHCl3:CH3OH 0.6 16 –1 27
3.31 ± 0.21 (medium) 12 7.3:1 CHCl3:CH3OH 0.8 24 −2 26
6.73 ± 0.51 (thick) 12 CHCl3 0.8 24 −2 26

Abbreviation: PCL, poly(ε‐caprolactone).