Skip to main content
. 2021 Mar 10;13(6):851. doi: 10.3390/polym13060851

Table 2.

First TGA mass loss at 160 °C and temperatures corresponding to 5% and 10% weight loss for untreated and treated hemp fibers.

Sample First Mass Loss (%) at 160 °C T5 (°C) T10 (°C)
Uf 1.4 254 289
Wf 0.3 272 299
WSf 0.3 278 305
Af 0.3 292 313
ASf 0.3 288 310