. 2021 Mar 10;14(6):1324. doi: 10.3390/ma14061324

Figure 3.

Figure 3

Results of mechanical tests performed in compression mode on CaCO3-filled E57/TFF/100:22 specimens after different immersion times (i.e., 1, 6, and 10 months) in demineralized water, in terms of (a) Compressive modulus; (b) Compressive maximum strength; (c) Compressive strain at break.