Material Average Hardness Impact Energy (J) Elongation at Break (%)
St52/S355J2G3/S355JR 180 HB 27 (−20 °C) 22
E355
S275JR 160 HB 27 (20 °C) 22
S235JR 140 HB 27 (20 °C) 26
BS970070M20 140 HB 24 (10 °C) 21
R35 112 HB 27 (0 °C) 24
R45 142 HB 22 (20 °C) 22
IS 1030 GRADE 280-580 220 HB 22 (20 °C) 18
AISI 304 215 HB 60 (−196 °C) 45
60-40-18 160 HB 12 (−20 °C) 18
Al 7075-T6 150 HB 17 (23 °C) 10
POM 81 (Shore D) - 30
PA 76–82 (Shore D) - 20–200
PP 70–83 (Shore D) - 150–600