Table 2.
Figure Number | Sample | Composition (Treatment 1) | 2θ, Degree | D, nm | Structure Signal |
---|---|---|---|---|---|
a | 1 | ZnO NPs-PEG | 36.18 | 14.040 | ZnO (wurtzite) |
47.60 | 11.562 | ||||
56.54 | 12.285 | ||||
b | 2 | BC | 22.96 | 4.749 | BC |
c | 3 | BC (film)–ZnO NPs | 22.68 | 4.601 | BC |
36.38 | 18.719 | ZnO (wurtzite) | |||
47.80 | 18.284 | ||||
56.84 | 15.725 | ||||
d | 4 | BC–ZnO NPs | 23.08 | 5.520 | BC |
36.64 | 10.620 | ZnO (wurtzite) | |||
- | - | ZnO NPs 2 | 31.76 | 11.600 | ZnO (wurtzite) |
34.36 | 17.500 | ||||
36.22 | 11.700 |
1 Ultrasound treatment. 2 Data of our samples protected by betulin diphosphate (BDP) were published in [3].