Data of powder XRD patterns of BC-ZnO NPs samples (Figure 1).

Figure Number Sample Composition (Treatment 1) 2θ, Degree D, nm Structure Signal
a 1 ZnO NPs-PEG 36.18 14.040 ZnO (wurtzite)
47.60 11.562
56.54 12.285
b 2 BC 22.96 4.749 BC
c 3 BC (film)–ZnO NPs 22.68 4.601 BC
36.38 18.719 ZnO (wurtzite)
47.80 18.284
56.84 15.725
d 4 BC–ZnO NPs 23.08 5.520 BC
36.64 10.620 ZnO (wurtzite)
- - ZnO NPs 2 31.76 11.600 ZnO (wurtzite)
34.36 17.500
36.22 11.700

1 Ultrasound treatment. 2 Data of our samples protected by betulin diphosphate (BDP) were published in [3].