Skip to main content
. 2021 Mar 11;14(6):1360. doi: 10.3390/ma14061360

Figure 1.

Figure 1

The XRD patterns of MgCa4.5Gd0.5 and MgCa4.5 after micro-arc oxidation (MAO) process done under 140 V and 120 V.