Skip to main content
. 2021 Mar 11;14(6):1360. doi: 10.3390/ma14061360

Figure 4.

Figure 4

SEM image of the MgCa4.5 alloy sample morphology after MAO process under 140 V: (a) magnification 500×, (b) magnification 5000× and EDS spectra of (c) pores, (d) grooves.