. 2021 Mar 10;13(6):854. doi: 10.3390/polym13060854

Table 1.

Tensile properties of PCL/Gel blend nanofiber containing 0–2% EPS.

Sample Modulus (MPa) Tensile Strength (MPa) Elongation at Break (%)
PCL/Gel 135 ± 10 6.23 ± 0.20 28.2 ± 3.0
PCL/Gel + 1% EPS 116 ± 12 6.01 ± 0.69 19.6 ± 5.1
PCL/Gel + 2% EPS 137 ± 13 6.17 ± 0.20 14.0 ± 3.5