Figure 7.

Figure 7

HRTEM micrographs of uncoated and coated samples: (A) Uncoated Fe3O4 nanoparticles (50 nm bar); (C) FPVAFU-ZLDH (50 nm bar); and (B,D) show their particle size distribution, respectively.