(A) TEM micrograph of PLGA nanoparticles prepared by using 3 mg of sclareol (SCL); bar = 200 nm. (B) Mean sizes of PLGA nanoparticles prepared by using 3 mg of cholesterol (Chol) or sclareol (SCL) and then coated with hyaluronic acid (HA). (C) Entrapment efficiency of SCL as a function of the amount of active compound used during the preparation of PLGA nanoparticles. (D) Evaluation of the amount of HA adsorbed on the surface of PLGA nanoparticles prepared with 3 mg of SCL as a function of the amount of polysaccharide used. Reprinted with permission from [7]. Copyright ©2019 Elsevier Ltd.