. 2020 Jul 22;12(35):39549–39560. doi: 10.1021/acsami.0c09178

Figure 4.

Figure 4

Impedance (a) Bode and (b) complex plane plots recorded for glassy carbon, GO, pure SnO2, 32:1 SnO2–GO, and mechanically mixed SnO2 + GO recorded in 0.1 M phosphate-buffered saline (PBS) at −0.15 V (potential at which the adopted probe, [Ru(NH3)6]Cl3, is oxidized). Points are the experimental values, while continuous lines are the simulated data according to the equivalent circuits, shown in (c).