Skip to main content
. 2021 Mar 26;13(7):1043. doi: 10.3390/polym13071043

Figure 3.

Figure 3

(a) Voltammograms, recorded during oxidation and reduction processes (v = 0.1 V/s; 0.1 M Bu4NPF6/ACN) of studied oligo- and polyazomethine thin films, deposited on the glass with ITO together with voltammogram obtain for PAz-BOO-Oct, presented previously in [11]; (b) the energy levels of HOMO and LUMO orbitals, designated based on the results of cyclic voltammetry measurements.