. 2021 Mar 25;22(7):3350. doi: 10.3390/ijms22073350

Figure 4.

Figure 4

Thickness measurement of produced ASC-based self-assembled scaffold under hypoxic condition using 50, 100 and 200 μg/mL concentrations of ascorbic acid. The graph shows mean measurements ± SEM. The reading of thickness measurement for each of the self-assembled scaffolds was repeated in five predetermined positions (technical replicate). The results are representative of measurements from three biologically independent samples. * Represents statistically significant difference using paired t test (p < 0.05).