Images of flank wears gradually emerge on HSS, HSS-TiN, and HSS-Co under a microscope magnification scale from 30× to150×.

Tools Cutting Speed (rpm) Initial Condition Final Condition (25th Hole)
HSS 250 graphic file with name materials-14-01628-i001.jpg graphic file with name materials-14-01628-i002.jpg
100 graphic file with name materials-14-01628-i003.jpg graphic file with name materials-14-01628-i004.jpg
HSS-TiN 250 graphic file with name materials-14-01628-i005.jpg graphic file with name materials-14-01628-i006.jpg
100 graphic file with name materials-14-01628-i007.jpg graphic file with name materials-14-01628-i008.jpg
HSS-Co 250 graphic file with name materials-14-01628-i009.jpg graphic file with name materials-14-01628-i010.jpg
100 graphic file with name materials-14-01628-i011.jpg graphic file with name materials-14-01628-i012.jpg