Skip to main content
. 2021 Mar 24;13(7):999. doi: 10.3390/polym13070999

Figure 9.

Figure 9

SEM micrographs of the HDPE MPs after visible-light photocatalytic degradation for 50 h by C,N-TiO2 in the (a) tert-Butanol, (b) isopropyl alcohol (c) tiron, and (d) copper nitrate scavengers.