Glass transition temperature (Tg) and decomposition temperature (Td) [endothermic peaks] of 10 wt % electrospun PAN-MA/lignin nanofibers.

Sample ID Tg, °C Td (Exo), °C
PAN-MA 97.4 309.1
AL-1 98.0 311.6
AL-2 97.4 314.4
LSL-1 98.4 299.7
LSL-2 99.9 281.5