Table 5.
Physical State | Tg(°C) | Tonset(°C) | Td5%(°C) | Td10%(°C) | Tpeak(°C) | Ref. | |
---|---|---|---|---|---|---|---|
78a | Glass | −21 1,2 | --- | --- | 231 3 | --- | [68] |
78b | Viscous material | −68 1,2 | --- | --- | 232 3 | --- | [68] |
78c | Viscous material | −51 1,2 | --- | --- | 229 3 | --- | [68] |
78d | Viscous material | −60 1,2 | --- | --- | 245 3 | --- | [68] |
80a | Glass | −8 1,2 | --- | --- | 238 3 | --- | [68] |
80b | Viscous material | −27 1,2 | --- | --- | 250 3 | --- | [68] |
80c | Viscous material | −37 1,2 | --- | --- | 251 3 | --- | [68] |
80d | Viscous material | −58 1,2 | --- | --- | 269 3 | --- | [68] |
83a | Yellow solid | --- | 219.6 4,5 336.5 4,6 |
218.3 4 | 226.9 4 | 238.6 4,5 363.5 4,6 |
[70] |
83b | Orange solid | --- | 222.3 4,5 | 223.0 4 | 228.7 4 | 277.1 4,5 349.5 4,6 |
[70] |
84a | Yellow solid | --- | 181.8 4,5 227.4 4,6 |
192.2 4 | 228.4 4 | 192.2 4,5 246.1 4,6 353.1 4,7 |
[70] |
84b | Brick red solid | 79.9 8 | 233.7 4 | 216.1 4 | 228.9 4 | 288.8 4 | [70] |
85a | Yellow orange glassy solid | 49.3 8 | 370.7 4 | 358.3 4 | 370.8 4 | 391.7 4 | [70] |
85b | Pale yellow glassy solid | 31.4 8 | 354.3 4 | 347.8 4 | 357.03 4 | 366.4 4,5 382.4 4,6 |
[70] |
86a | Brick red glassy solid | 48.1 8 | 370.1 4 | 362.5 4 | 372.2 4 | 394.8 4 | [70] |
86b | Pale brown glassy solid | 28.4 8 | 370.5 4 | 356.7 4 | 376.6 4 | 387.5 4 | [70] |
1 DSC conditions: 20 °C/min, He; 2 Measured during the second heating cycle; 3 TGA conditions: 20 °C/min to 600 °C, N2; 4 TGA conditions: 10 °C/min from 40 °C to 900 °C, N2, Pt pan (100 μL). Every sample was dried in the furnace at 60 °C for 10 min under an N2 atmosphere prior to measurement; 5 Referred to the first degradation event; 6 Referred to the second degradation event; 7 Referred to the third degradation event; 8 DSC conditions: The samples were heated to the maximal temperature (10 °C/min) to remove thermal history, then cooled to −90 °C (5 °C/min) and heated from −90 °C to the maximal temperature (10 °C/min) (the two heating ramps lead to the same results), dry N2 (30 cm3/min), 1.44–7.21 mg, aluminum pan with a pinhole on the cap, the maximal temperature was 180 °C for 83a,b, 84a,b, 300 °C for 83c and 84c, 250 °C for 83d and 210 °C for 84d.