Skip to main content
. 2021 Apr 4;14(7):1780. doi: 10.3390/ma14071780

Figure 5.

Figure 5

(a) An example of a thin diamond film grown on silicon. After the thinning of the silicon wafer up to a thickness of about 80 µm, substrate bending is clearly evidenced. (b) 5 mm × 5 mm diamond on 120 µm thick silicon plates after membrane fabrication.