Skip to main content
. 2021 Apr 5;13(7):1167. doi: 10.3390/polym13071167

Table 1.

Processing conditions in the twin screw extruder for the formulation of all the nanocomposites.

Polymer Matrix Temperature Profile (°C) Screw Rotation Speed (rpm)
MB1 90-11 -130-140-140-150-150 205
MB2 90-110-130-140-140-145 -145 220
LDPE 110-120-140-160-170-180-180 220