Figure 8.

Figure 8

(a) Top-view images of the CMC–PAA-based (up) and SH-based (down) BP anode before and after cycling; (b) cross-sectional SEM images of the pristine SH-based BP anode (up), and of the same electrode observed after the end of galvanostatic cycling tests (down).