(a) Photographs of hole drilling and water-jet cutting processes, and we have found that a pre-drilled hole with a diameter of 2 mm and then expanded to 10 mm using water-jet leaves no cracks and delamination around the hole in the specimen. (b) Open-hole specimen geometry and four-point bending experimental setup.