Table 1.
Films | T280 (%) | T660 (%) | WVP (×10−9 g·m/m2·Pa·s) |
---|---|---|---|
CNF | 68.89 ± 0.30 d | 89.05 ± 0.93 c | 0.55 ± 0.02 b |
CNF/ZnO | 35.23 ± 1.98 a | 81.57 ± 1.51 a | 0.46 ± 0.01 a |
CNF/GSE | 57.75 ± 0.82 c | 87.48 ± 0.30 c | 0.56 ± 0.05 b |
CNF/ZnO/GSE | 44.75 ± 2.14 b | 84.32 ± 0.79 b | 0.51 ± 0.01 ab |
* Data with the same superscript letter within the same column are not significantly (p > 0.05) different from Duncan’s multiple range tests.